High-Nickel Lithium Battery Runaway Tamed

Google+ Pinterest LinkedIn Tumblr +

A high nickel concentration in lithium-ion batteries could be a bonus for mobility devices, if we could contain the risk of thermal runaway. This potentially catastrophic event occurs after traditional organic liquid electrolyte overheats, or a short-circuit occurs inside a battery. But now, researchers from Republic of Korea may have finally resolved this high-nickel lithium battery drawback.

Safety in High-Nickel Lithium Batteries

Scientists from four academic institutions gathered together, to write the report we link to below.  They were concerned about the safety of lithium-ion batteries, especially since their demand seemed never-ending to them.

They were aware of the potential of high-nickel lithium battery chemistry for electric vehicles, and other mobility devices. And so they set their minds to addressing the significant potential of these high-density batteries to catch fire.

Before the scientists began their work, they noted that broad scientific interest was focussed on enhancing the driving range of electric vehicles. And that this in turn necessitated improving the ability of lithium-ion batteries to store energy.

This high-profile need motivated the researchers’ interest in energy-dense high-nickel chemistry. The team from Republic of Korea decided to find a way to avert thermal runaway in these otherwise promising batteries.

How the Scientists Improved the Recipe

The scientists believed their solution lay in replacing the traditional liquid electrolyte, with a new, non-flammable one. But first, they needed to develop a thermally durable interphase at the cathode and anode interfaces.

They derived their non-flammable liquid electrolyte from a fluorinated-carbonate, and standard lithium salt-based concentration.This delivered the stable, non-flammable result they needed.

But they achieved a second, perhaps unexpected bonus. Their prototype high-nickel lithium battery pouch-cell achieved 600 charge-discharge cycles at one degree centigrade. At that point it still retained 81% of its original capacity, without a sign of any lithium dendrites!

More Information

Pathway to Safer Nickel Batteries in Texas

Lithium Nickel Oxide Degradation Discovery

Preview Image: Modified Battery Averts Thermal Runaway

Report on Preventing Thermal Runaway

Share.

About Author

Electricity has always intrigued me. I have been writing about batteries and energy storage for more than ten years, and have published over 4,000 articles on this website. During that time, I have researched developments across lead-acid, lithium-ion, sodium-ion, flow batteries, and emerging energy-storage technologies. My goal is to explain complex battery concepts in clear, practical language that anyone can understand. My writing career began unexpectedly after leaving the corporate world. What started as a search for a new direction gradually became a fascination with batteries, renewable energy, and the science that powers modern life. Writing may not have made me wealthy, but it has given me the opportunity to explore an industry that continues to evolve in remarkable ways.

Leave A Reply